Exploració per tema "Y-TZP"
Ara es mostren els items 1-3 de 3
-
Annealing aged zirconia: study of surface mechanical properties at the micrometric length scale
(Elsevier, 2015-03-01)
Article
Accés obertThe annealing of hydrothermal aged zirconia has been studied by analysing the changes in microstructure and surface mechanical properties in terms of the annealing temperature. In this experimental work, a systematic micro- ... -
Hydrofluoric acid etching of dental zirconia. Part 2: effect on flexural strength and ageing behavior
(Elsevier, 2016-01-01)
Article
Accés obertAmong the diverse treatments proposed to promote the osseointegration of zirconia dental implants, hydrofluoric acid (HF) etching appears to be a good candidate. However little is known on the effect of this process on the ... -
Weibull strength statistics of hydrothermally aged 3 mol% yttria-stabilised tetragonal zirconia
(2014-09-01)
Article
Accés restringit per política de l'editorialThe effect of hydrothermal degradation on the flexural strength and on the fracture statistics of 3 mol% yttria-stabilized tetragonal zirconia (3Y-TZP) has been investigated. To do so, a large number ( > 30) of specimens ...