Processing and characterization of high-density zirconia-carbon nanotube composites
Visualitza/Obre
processing.pdf (1,774Mb) (Accés restringit)
Sol·licita una còpia a l'autor
Què és aquest botó?
Aquest botó permet demanar una còpia d'un document restringit a l'autor. Es mostra quan:
- Disposem del correu electrònic de l'autor
- El document té una mida inferior a 20 Mb
- Es tracta d'un document d'accés restringit per decisió de l'autor o d'un document d'accés restringit per política de l'editorial
Cita com:
hdl:2117/16659
Tipus de documentArticle
Data publicació2012-07-15
Condicions d'accésAccés restringit per política de l'editorial
Llevat que s'hi indiqui el contrari, els
continguts d'aquesta obra estan subjectes a la llicència de Creative Commons
:
Reconeixement-NoComercial-SenseObraDerivada 3.0 Espanya
Abstract
Addition of multiwall carbon nanotubes (MWCNTs) to polycrystalline ceramics is currently considered as a potential method for improving their mechanical properties, mainly their fracture toughness. High density composites produced by the addition of relatively small volume fractions of MWCNTs (0–2 vol.%) to 3 mol% yttria doped zirconia (3Y-TZP) have been produced by spark plasma sintering, resulting in a homogeneous distribution of MWCNTs with a small average matrix grain size in the range 153–182 nm. The influence of transformation toughening is found to be very weak for this small grain size by measuring the extent of phase transformation in the crack wake. Also, no hydrothermal degradation takes place after more than 200 h at 131 °C either in the monolithic ceramic or in the composites. The study of the influence of MWCNTs on the microstructure and mechanical properties of 3Y-TZP shows that in the composites there is a very slight decrease in hardness, while the elastic modulus does not practically change. By fitting the crack opening displacement in the near crack tip region to the Irwin parabola, the intrinsic fracture toughness is found to be approximately the same in the matrix and in the 2 vol.% composites. In spite of the observation of some crack bridging by nanotubes, from the measurement of the crack opening displacement (δ) along the crack faces, it is concluded that there is hardly any change in δ in 3Y-TZP by the addition of 2 vol.% of MWCNTs not only in the crack tip region but also in all the range studied. However, the indentation fracture toughness is nearly 15% higher in 2 vol.% composites as compared to their monolithic counterparts.
CitacióChintapalli, R. [et al.]. Processing and characterization of high-density zirconia-carbon nanotube composites. "Materials science and engineering A. Structural materials properties microstructure and processing", 15 Juliol 2012, vol. 549, p. 50-59.
ISSN0921-5093
Versió de l'editorhttp://www.sciencedirect.com/science/article/pii/S0921509312005242#
Fitxers | Descripció | Mida | Format | Visualitza |
---|---|---|---|---|
processing.pdf | 1,774Mb | Accés restringit |