Citació: Chintapalli, R. [et al.]. Processing and characterization of high-density zirconia-carbon nanotube composites. "Materials science and engineering A. Structural materials properties microstructure and processing", 15 Juliol 2012, vol. 549, p. 50-59.
Títol: Processing and characterization of high-density zirconia-carbon nanotube composites
Autor: Chintapalli, R.K.; García Marro, Fernando Veure Producció científica UPC; Milsom, Ben; Reece, Michel; Anglada Gomila, Marcos Juan Veure Producció científica UPC
Data: 15-jul-2012
Tipus de document: Article
Resum: Addition of multiwall carbon nanotubes (MWCNTs) to polycrystalline ceramics is currently considered as a potential method for improving their mechanical properties, mainly their fracture toughness. High density composites produced by the addition of relatively small volume fractions of MWCNTs (0–2 vol.%) to 3 mol% yttria doped zirconia (3Y-TZP) have been produced by spark plasma sintering, resulting in a homogeneous distribution of MWCNTs with a small average matrix grain size in the range 153–182 nm. The influence of transformation toughening is found to be very weak for this small grain size by measuring the extent of phase transformation in the crack wake. Also, no hydrothermal degradation takes place after more than 200 h at 131 °C either in the monolithic ceramic or in the composites. The study of the influence of MWCNTs on the microstructure and mechanical properties of 3Y-TZP shows that in the composites there is a very slight decrease in hardness, while the elastic modulus does not practically change. By fitting the crack opening displacement in the near crack tip region to the Irwin parabola, the intrinsic fracture toughness is found to be approximately the same in the matrix and in the 2 vol.% composites. In spite of the observation of some crack bridging by nanotubes, from the measurement of the crack opening displacement (δ) along the crack faces, it is concluded that there is hardly any change in δ in 3Y-TZP by the addition of 2 vol.% of MWCNTs not only in the crack tip region but also in all the range studied. However, the indentation fracture toughness is nearly 15% higher in 2 vol.% composites as compared to their monolithic counterparts.
ISSN: 0921-5093
URI: http://hdl.handle.net/2117/16659
DOI: 10.1016/j.msea.2012.03.115
Versió de l'editor: http://www.sciencedirect.com/science/article/pii/S0921509312005242#
Apareix a les col·leccions:Altres. Enviament des de DRAC
CIEFMA - Centre d'Integritat Estructural i Fiabilitat dels Materials. Articles de revista
Departament de Ciència dels Materials i Enginyeria Metal·lúrgica. Articles de revista
Comparteix:


Stats Mostra les estadístiques d'aquest ítem

SFX Query

Aquest ítem (excepte textos i imatges no creats per l'autor) està subjecte a una llicència de Creative Commons Llicència Creative Commons
Creative Commons

 

Valid XHTML 1.0! Programari DSpace Copyright © 2002-2004 MIT and Hewlett-Packard Comentaris
Universitat Politècnica de Catalunya. Servei de Biblioteques, Publicacions i Arxius