Citació: Macanás, J. [et al.]. Hydrogen generation by aluminum corrosion in aqueous alkaline solutions of inorganic promoters: the Alhidrox process. "Energy", Maig 2011, vol. 36, núm. 5, p. 2493-2501.
Títol: Hydrogen generation by aluminum corrosion in aqueous alkaline solutions of inorganic promoters: the Alhidrox process
Autor: Macanás de Benito, Jorge Veure Producció científica UPC; Soler Turu, Lluis; Candela Soto, Angélica Maria; Muñoz Tapia, Maria; Casado Giménez, Juan
Data: mai-2011
Tipus de document: Article
Resum: The research of alternative processes to obtain clean fuels has become a main issue because of the concerns related to the current energy system, both from economical and environmental points of view. Hydrogen storage and production methods are being investigated for stationary and portable applications. Up to now, a significant part of H2 production on demand was thought to be fulfilled by using chemical hydrides, but recent studies have proved the limitations of this approach. Conversely, H2 production based in the corrosion of light metals in water solutions is an interesting alternative. Among all of them, Al is probably the most adequate metal for energetic purposes due to its high electron density and oxidation potential. But concerning H2 production from Al corrosion in water, a major issue remains unsolved: metal passivation due to the formation of Al(OH)3 inhibits H2 evolution. In this work we show the last results obtained for the generation of H2 from water using Al powder using diverse alkaline solutions. It is confirmed that corrosion is not affected solely by the solution pH but also by the nature of the ionic species found in the aqueous medium. Moreover, we describe the AlHidrox process, which minimizes Al passivation under mild conditions by the addition of different inorganic salts as corrosion promoters, allowing 100% yields and flow rates up to 2.9 L/min per gram of Al. The feasibility of the process has been regarded in terms of stability (by conducting several successive runs) and selfinitiation without an external heating.
ISSN: 0360-5442
URI: http://hdl.handle.net/2117/12541
DOI: 10.1016/j.energy.2011.01.041
Apareix a les col·leccions:Altres. Enviament des de DRAC
POLQUITEX - Materials Polimérics i Química Téxtil. Articles de revista
Departament d'Enginyeria Química. Articles de revista
Comparteix:


Stats Mostra les estadístiques d'aquest ítem

SFX Query

Tots els drets reservats. Aquesta obra està protegida pels drets de propietat intel·lectual i industrial corresponents. Sense perjudici de les exempcions legals existents, queda prohibida la seva reproducció, distribució, comunicació pública o transformació sense l'autorització del titular dels drets.

Per a qualsevol ús que se'n vulgui fer no previst a la llei, dirigiu-vos a: sepi.bupc@upc.edu

 

Valid XHTML 1.0! Programari DSpace Copyright © 2002-2004 MIT and Hewlett-Packard Comentaris
Universitat Politècnica de Catalunya. Servei de Biblioteques, Publicacions i Arxius